1.1 This specification2 covers austenitic steel castings for valves, flanges, fittings, and other pressure-containing parts (Note 1). Note 1—Carbon steel castings for pressure-containing parts are covered by Specification A216/A216M, low-alloy steel castings by Specification A217/A217M, and duplex stainless steel castings by Specification A995/A995M. 1.2 A number of grades of austenitic steel castings are included in this specification. Since these grades possess varying degrees of suitability for service at high temperatures or in corrosive environments, it is the responsibility of the purchaser to determine which grade shall be furnished. Selection will depend on design and service conditions, mechanical properties, and high-temperature or corrosion-resistant characteristics, or both. 1.2.1 Because of thermal instability, Grades CE20N, CF3A, CF3MA, and CF8A are not recommended for service at temperatures above 800°F [425°C]. 1.3 Supplementary requirements of an optional nature are provided for use at the option of the purchaser. The Supplementary requirements shall apply only when specified individually by the purchaser in the purchase order or contract. 1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.4.1 This specification is expressed in both inch-pound units and in SI units; however, unless the purchase order or contract specifies the applicable M specification designation (SI units), the inch-pound units shall apply. Within the text, the SI units are shown in brackets or parentheses.

Standard Specification for Castings, Austenitic, for Pressure-Containing Parts

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2013
实施

1.1 This specification covers a group of cast duplex stainless steels (austenitic/ferritic). 1.2 The duplex stainless steel alloys offer a combination of enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated. Ferrite levels are not specified, but these alloys will develop a range of approximately 30 to 608201;% ferrite with the balance austenite. It is the responsibility of the purchaser to determine which grade shall be furnished depending on design and service conditions, mechanical properties, and corrosion-resistant characteristics.Note 1—Because of the possibility of precipitation of embrittling phases, the grades included in this specification are not recommended for service at temperatures above 600ºF [315ºC]. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.3.1 Within the text, the SI units are shown in brackets.

Standard Specification for Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application

ICS
77.140.80 (Iron and steel castings)
CCS
发布
2013
实施

1.1 This specification covers alloy steel castings, which have been subjected to special heat treatment, for valves, flanges, fittings, and other pressure-containing parts (Note 1) intended primarily for high-temperature service. 1.2 The high-temperature properties of the materials covered in this specification are dependent upon special heat treatment that is required. Although the high-temperature properties are not specified, they are implied by control of chemistry, heat treatment, and room-temperature properties. 1.3 Two grades of ferritic alloy steel are covered (Note 2). Selection will depend on the design and service conditions, mechanical properties, and high-temperature characteristics. Note 1—Carbon steel castings for pressure-containing parts are covered by Specification A216/A216M. Alloy steel castings are covered by Specification A217/A217M. 8199;Note 2—The grades covered by this specification represent materials that are generally suitable for assembly with other castings or wrought steel parts by fusion welding. It is not intended to imply that these grades possess equal degrees of weldability; therefore, it is the responsibility of the purchaser to establish for himself a suitable welding technique. Since these grades possess varying degrees of suitability for resistance to oxidation and for high-temperature service, it is also the responsibility of the purchaser to determine which grade shall be furnished, due consideration being given to the requirements of the applicable construction codes. 1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

Standard Specification for Steel Castings, Alloy, Specially Heat-Treated, for Pressure-Containing Parts, Suitable for High-Temperature Service

ICS
77.140.80 (Iron and steel castings)
CCS
发布
2013
实施

1.1 This specification covers a group of requirements that are mandatory requirements of the following steel casting specifications issued by ASTM. If the product specification specifies different requirements, the product specification shall prevail. ASTM Designation 8201; Title of Specification A27/A27M Steel Castings, Carbon, for General Application A128/A128M Steel Castings, Austenitic Manganese A148/A148M Steel Castings, High Strength, for Structural Purposes A297/A297M Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant for General Application A447/A447M Steel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service A494/A494M Castings, Nickel and Nickel Alloy A560/A560M Castings, Chromium-Nickel Alloy A743/A743M Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application A744/A744M Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe A747/A747M Steel Castings, Stainless, Precipitation Hardening A890/A890M Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application A915/A915M Steel Castings, Carbon and Alloy, Chemical Requirements Similar to Standard Wrought Grades A958 Steel Castings, Carbon and Alloy, with Tensile Requirements, C......

Standard Specification for Castings, Steel and Alloy, Common Requirements, for General Industrial Use

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2013
实施

1.1 This specification covers a group of requirements that are mandatory requirements of the following steel casting specifications issued by ASTM. If the product specification specifies different requirements, the product specification shall prevail. ASTM Designation 8201; Title of Specification A27/A27M Steel Castings, Carbon, for General Application A128/A128M Steel Castings, Austenitic Manganese A148/A148M Steel Castings, High Strength, for Structural Purposes A297/A297M Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant for General Application A447/A447M Steel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service A494/A494M Castings, Nickel and Nickel Alloy A560/A560M Castings, Chromium-Nickel Alloy A743/A743M Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application A744/A744M Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe......

Standard Specification for Castings, Steel and Alloy, Common Requirements, for General Industrial Use

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2013
实施

1.1 This specification2 covers a group of common requirements that, unless otherwise specified in an individual specification, shall apply to steel castings for pressure-containing parts under each of the following ASTM specifications:   Title of Specification ASTM Designation       Steel Castings, Carbon, Suitable for Fusion Welding, A216/A216M   for High-Temperature Service   Steel Castings, Martensitic Stainless and Alloy, for A217/A217M   Pressure-Containing Parts, Suitable for High-     Temperature Service   Castings, Austenitic, Austenitic-Ferritic (Duplex), A351/A351M   Pressure-Containing Parts   Steel Castings, Ferritic and Martensitic, for Pressure- A352/A352M   Containing Parts, Suitable for Low-Temperature     Service

Standard Specification for Steel Castings, General Requirements, for Pressure-Containing Parts

ICS
77.140.80 (Iron and steel castings)
CCS
发布
2013
实施

1.1 This specification covers iron-chromium-nickel alloy, stainless steel castings intended for particularly severe corrosive applications. 1.2 This specification requires postweld heat-treatment of all weld repairs affecting surfaces intended to be wetted by the corrosive medium. For applications for which postweld heat-treatment is not considered mandatory for retention of acceptable corrosion resistance, refer to Specification A743/A743M. Note 1—For general corrosion-resistant alloy castings, reference should be made to Specification A743/A743M. For general heat-resistant alloy castings, reference should be made to Specification A297/A297M. For nickel-base alloy castings, refer to Specification A494/A494M. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.3.1 Within the text, the SI units are shown in brackets. 1.3.2 Inch-pound units are applicable for material ordered to Specification A744 and SI units for material ordered to Specification A744M.

Standard Specification for Castings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe Service

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2013
实施

1.1 This specification covers carbon steel castings for general applications that require up to 70 ksi (485 MPa) minimum tensile strength. Note 1—The grades covered by this specification represent materials that are suitable for assembly with other steel castings or wrought steel parts by fusion welding. It is not intended to imply that all these grades possess the same degree of weldability or that the same welding techniques can be used on all castings. It is the responsibility of the purchaser to establish for himself a suitable welding technique. 1.2 Several grades and two classes of steel castings are covered, as indicated below. The grade and class desired shall be specified by the purchaser. 1.2.1 Grade N-1—Chemical analysis only. 1.2.2 Grade N-2—Heat-treated but not mechanically tested. 1.2.3 Grade U-60-30 [415-205]—Mechanically tested but not heat-treated. 1.2.4 Grades 60-30  [415-205], 65-35 [450-240], 70-36 [485-250], and 70-40 [485-275]—Heat-treated and mechanically tested. 1.2.5 Class 1 and Class 2 steel castings shall be specified in accordance with 9.2. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.4 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Standard Specification for Steel Castings, Carbon, for General Application

ICS
77.140.80 (Iron and steel castings)
CCS
发布
2013
实施

1.1 This specification covers a group of cast duplex stainless steels (austenitic/ferritic). 1.2 The duplex stainless steel alloys offer a combination of enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated. Ferrite levels are not specified, but these alloys will develop a range of approximately 30 to 60 % ferrite with the balance austenite. It is the responsibility of the purchaser to determine which grade shall be furnished depending on design and service conditions, mechanical properties, and corrosion-resistant characteristics. Note 18212;Because of the possibility of precipitation of embrittling phases, the grades included in this specification are not recommended for service at temperatures above 600ºF [315ºC]. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.3.1 Within the text, the SI units are shown in brackets.

Standard Specification for Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application

ICS
77.140.80 (Iron and steel castings)
CCS
J31;H40
发布
2012
实施

1.1 This specification2 covers martensitic stainless steel and alloy steel castings for valves, flanges, fittings, and other pressure-containing parts (Note 1) intended primarily for high-temperature and corrosive service (Note 2). 1.2 One grade of martensitic stainless steel and nine grades of ferritic alloy steel are covered. Selection will depend on design and service conditions, mechanical properties, and the high-temperature and corrosion-resistant characteristics (Note 3). Note 1???Carbon steel castings for pressure-containing parts are covered by Specification A216/A216M. Low alloy quench-and-tempered grades equivalent to Specification A217/A217M grades may be found in both Specifications A352/A352M and A487/A487M. Note 2???The grades covered by this specification represent materials that are generally suitable for assembly with other castings or wrought steel parts by fusion welding. It is not intended to imply that these grades possess equal degrees of weldability; therefore, it is the responsibility of the purchaser to establish for himself a suitable welding technique. Since these grades possess varying degrees of suitability for high-temperature and corrosion-resistant service, it is also the responsibility of the purchaser to determine which grade shall be furnished, due consideration being given to the requirements of the applicable construction codes.Note 3???The committee formulating this specification has included nine grades of materials that are considered to represent basic types of ferritic alloy steels suitable for valves, flanges, fittings, and other pressure-containing parts. Additional alloy steels that may better fulfill certain types of service will be considered for inclusion in this specification by the committee as the need becomes apparent. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

Standard Specification for Steel Castings, Martensitic Stainless and Alloy, for Pressure-Containing Parts, Suitable for High-Temperature Service

ICS
77.140.80 (Iron and steel castings)
CCS
H40
发布
2012
实施

1.1 This specification covers a group of cast duplex stainless steels (austenitic/ferritic). 1.2 The duplex stainless steel alloys offer a combination of enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated. Ferrite levels are not specified, but these alloys will develop a range of approximately 30 to 608201;% ferrite with the balance austenite. It is the responsibility of the purchaser to determine which grade shall be furnished depending on design and service conditions, mechanical properties, and corrosion-resistant characteristics.Note 1???Because of the possibility of precipitation of embrittling phases, the grades included in this specification are not recommended for service at temperatures above 600??F [315??C]. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.3.1 Within the text, the SI units are shown in brackets.

Standard Specification for Castings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application

ICS
77.140.80 (Iron and steel castings)
CCS
J31;H40
发布
2012
实施

1.1 This specification covers a group of requirements that are mandatory requirements of the following steel casting specifications issued by ASTM. If the product specification specifies different requirements, the product specification shall prevail. ASTM Designation Title of Specification A27/A27MSteel Castings, Carbon, for General Application A128/A128MSteel Castings, Austenitic Manganese A148/A148MSteel Castings, High Strength, for Structural Purposes A297/A297M Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant for General Application A447/A447MSteel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service A494/A494MCastings, Nickel and Nickel Alloy A560/A560MCastings, Chromium-Nickel Alloy A743/A743MCastings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application A744/A744MCastings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe A747/A747M Steel Castings, Stainless, Precipitation Hardening A890/A890MCastings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application A915/A915MSteel Castings, Carbon and Alloy, Chemical Requirements Similar to Standard Wrought Grades A958Steel Castings, Carbon and Alloy, with Tensile Requirements, Chemical Requirements Similiar to Standard Wrought Grades A1002Castings, Nickel-Aluminum Ordered Alloy 1.2 This ......

Standard Specification for Castings, Steel and Alloy, Common Requirements, for General Industrial Use

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施

1.1 This specification covers iron-chromium-nickel-copper corrosion-resistant steel castings, capable of being strengthened by precipitation hardening heat treatment. 1.2 These castings may be used in services requiring corrosion resistance and high strengths at temperatures up to 600°F [315°C]. They may be machined in the solution-annealed condition and subsequently precipitation hardened to the desired high-strength mechanical properties specified in Table S14.1 with little danger of cracking or distortion. 1.3 The material is not intended for use in the solution-annealed condition. Note 18212;If the service environment in which the material is to be used is considered conducive to stress-corrosion cracking, precipitation hardening should be performed at a temperature that will minimize the susceptibility of the material to this type of attack. 1.4 Supplementary requirements of an optional nature are provided for use at the option of the purchaser. The Supplementary requirements shall apply only when specified individually by the purchaser in the purchase order or contract. 1.5 This specification is expressed in both inch-pound units and in SI units; however, unless the purchase order or contract specifies the applicable M specification designation (SI units), the inch-pound units shall apply. 1.6 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.6.1 Within the text, the SI units are shown in brackets.

Standard Specification for Steel Castings, Stainless, Precipitation Hardening

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施

1.1 This specification covers austenitic-ferritic (duplex) stainless steel castings for valves, flanges, fittings, and other pressure-containing parts. 1.2 The duplex stainless steels offer a combination of enhanced mechanical properties and corrosion resistance when properly balanced in composition and properly heat treated. Ferrite levels are not specified, but these grades will develop a range of approximately 30 to 60 % ferrite with the balance austenite. It is the responsibility of the purchaser to determine which grade shall be furnished depending on design and service conditions, mechanical properties, and corrosion-resistant characteristics. Note 18212;Because of the possibility of precipitation of embrittling phases, the grades included in this specification are not recommended for service at temperatures above 600°F [315°C]. 1.3 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

Standard Specification for Castings, Austenitic-Ferritic (Duplex) Stainless Steel, for Pressure-Containing Parts

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施

1.1 This specification covers austenitic steel castings for valves, flanges, fittings, and other pressure-containing parts (Note 1). Note 18212;Carbon steel castings for pressure-containing parts are covered by Specification A216/A216M, low-alloy steel castings by Specification A217/A217M, and duplex stainless steel castings by Specification A995/A995M. 1.2 A number of grades of austenitic steel castings are included in this specification. Since these grades possess varying degrees of suitability for service at high temperatures or in corrosive environments, it is the responsibility of the purchaser to determine which grade shall be furnished. Selection will depend on design and service conditions, mechanical properties, and high-temperature or corrosion-resistant characteristics, or both. 1.2.1 Because of thermal instability, Grades CE20N, CF3A, CF3MA, and CF8A are not recommended for service at temperatures above 800°F [425°C]. 1.2.2 Because of embrittlement phases, Grade CD4MCu is not recommended for service at temperatures above 600°F [316°C]. 1.3 Supplementary requirements of an optional nature are provided for use at the option of the purchaser. The Supplementary requirements shall apply only when specified individually by the purchaser in the purchase order or contract. 1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.4.1 This specification is expressed in both inch-pound units and in SI units; however, unless the purchase order or contract specifies the applicable M specification designation (SI units), the inch-pound units shall apply. Within the text, the SI units are shown in brackets or parentheses.

Standard Specification for Castings, Austenitic, for Pressure-Containing Parts

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施

1.1 This specification2 covers a group of common requirements that, unless otherwise specified in an individual specification, shall apply to steel castings for pressure-containing parts under each of the following ASTM specifications: Title of Specification ASTM Designation Steel Castings, Carbon, Suitable for Fusion Welding, A216/A216M for High-Temperature Service Steel Castings, Martensitic Stainless and Alloy, for A217/A217M Pressure-Containing Parts, Suitable for High- Temperature Service Castings, Austenitic, Austenitic-Ferritic (Duplex), A351/A351M Pressure-Containing Parts Steel Castings, Ferritic and Martensitic, for Pressure- A352/A352M

Standard Specification for Steel Castings, General Requirements, for Pressure-Containing Parts

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施

1.1 This specification covers iron-chromium and iron-chromium-nickel alloy castings for general corrosion-resistant application. The grades covered by this specification represent types of alloy castings suitable for broad ranges of application which are intended for a wide variety of corrosion environments. Note 1???For alloy castings for severe corrosion-resistant service, reference should be made to Specification A744/A744M. For general heat-resistant alloy castings, reference should be made to Specification A297/A297M. For nickel alloy castings for corrosion-resistant service, reference should be made to Specification A494/A494M. 1.2 The values stated in either inch-pound units or SI units are to be regarded separately as standard. Within the text, the SI units are shown in brackets. The values stated in each system are not exact equivalents; therefore, each system must be used independently of the other. Combining values from the two systems may result in nonconformance with the specification. Inch-pound units are applicable for material ordered to Specification A743 and SI units for material ordered to Specification A743M.

Standard Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施

This test method is comparative and intended for use as a routine method to test materials for compliance with compositional specifications. It is assumed that all who use this test method will be trained analysts capable of performing common laboratory procedures skillfully and safely. It is expected that work will be performed in a properly equipped laboratory under appropriate quality control practices, such as those described in Guide E882.1.1 This test method covers the X-ray fluorescence spectrometric analysis of low-alloy steels and cast irons for the following elements in the ranges indicated: ElementsMass Fraction Range, % Manganese0.20 to 1.50 Nickel0.10 to 1.00 Chromium0.10 to 1.00 Molybdenum0.04 to 0.40 Copper0.05 to 0.30 Vanadium0.03 to 0.25 Note 18212;These mass fraction ranges can be extended by the use of suitable reference materials. The detection limit for the elements is lower than the listed minimum value. The ranges represent the actual levels at which this test method was tested. 1.2 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.

Standard Test Method for Analysis of Low-Alloy Steels and Cast Irons by Wavelength Dispersive X-Ray Fluorescence Spectrometry

ICS
77.140.80 (Iron and steel castings)
CCS
发布
2012
实施

1.1 This specification2 covers austenitic steel castings for valves, flanges, fittings, and other pressure-containing parts (Note 1). Note 1???Carbon steel castings for pressure-containing parts are covered by Specification A216/A216M, low-alloy steel castings by Specification A217/A217M, and duplex stainless steel castings by Specification A995/A995M. 1.2 A number of grades of austenitic steel castings are included in this specification. Since these grades possess varying degrees of suitability for service at high temperatures or in corrosive environments, it is the responsibility of the purchaser to determine which grade shall be furnished. Selection will depend on design and service conditions, mechanical properties, and high-temperature or corrosion-resistant characteristics, or both. 1.2.1 Because of thermal instability, Grades CE20N, CF3A, CF3MA, and CF8A are not recommended for service at temperatures above 800??F [425??C]. 1.3 Supplementary requirements of an optional nature are provided for use at the option of the purchaser. The Supplementary requirements shall apply only when specified individually by the purchaser in the purchase order or contract. 1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard. 1.4.1 This specification is expressed in both inch-pound units and in SI units; however, unless the purchase order or contract specifies the applicable M specification designation (SI units), the inch-pound units shall apply. Within the text, the SI units are shown in brackets or parentheses.

Standard Specification for Castings, Austenitic, for Pressure-Containing Parts

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施

1.1 This specification covers a group of requirements that are mandatory requirements of the following steel casting specifications issued by ASTM. If the product specification specifies different requirements, the product specification shall prevail. ASTM Designation Title of Specification A27/A27MSteel Castings, Carbon, for General Application A128/A128MSteel Castings, Austenitic Manganese A148/A148MSteel Castings, High Strength, for Structural Purposes A297/A297M Steel Castings, Iron-Chromium and Iron-Chromium-Nickel, Heat Resistant for General Application A447/A447MSteel Castings, Chromium-Nickel-Iron Alloy (25-12 Class), for High-Temperature Service A494/A494MCastings, Nickel and Nickel Alloy A560/A560MCastings, Chromium-Nickel Alloy A743/A743MCastings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application A744/A744MCastings, Iron-Chromium-Nickel, Corrosion Resistant, for Severe A747/A747M Steel Castings, Stainless, Precipitation Hardening A890/A890MCastings, Iron-Chromium-Nickel-Molybdenum Corrosion-Resistant, Duplex (Austenitic/Ferritic) for General Application A915/A915MSteel Castings, Carbon and Alloy, Chemical Requirements Similar to Standard Wrought Grades A958Steel Castings, Carbon and Alloy, with Tensile Requirements, Chemical Requirements Similiar to Standard Wrought Grades A1002Castings, Nickel-Aluminum Ordered Alloy 1.2 This ......

Standard Specification for Castings, Steel and Alloy, Common Requirements, for General Industrial Use

ICS
77.140.80 (Iron and steel castings)
CCS
J31
发布
2012
实施



Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号