H12 轻金属及其合金分析方法 标准查询与下载



共找到 784 条与 轻金属及其合金分析方法 相关的标准,共 53

本部分规定了电感耦合等离子体发汞光谱法测定硅钙合金中磷含量。 本部分适用于硅钙合金中磷含量的测定测正范 (质童分数)=0〉005%~0′08O%。

Determination of Phosphorus Content in Silicon Calcium Alloy Inductively Coupled Plasma Emission Spectrometry

ICS
CCS
H12
发布
2008-09-01
实施
2008-09-01

本标准规定了氧化铝中钠、钾、钙、硅、铁、钛、锰、锌、铜、钒、铬、硼等12种元素的方法。 本标准适用于氧化铝中钠、钾、钙、硅、铁、钛、锰、锌、铜、钒、铬、硼等12种元素含量的测定。测定范围含量如表1所示。

Determination of impurities in alumina.Inductively coupled plasma atomic emission spectrometric method (ICP-AES) with microwave dissolution

ICS
CCS
H12
发布
2008-04-29
实施
2008-11-01

本部分规定了高纯铝中钛含量的测定方法。 本部分适用于高纯铝中钛含量的测定。测定范围:0.00003%~0.00020%。

Chemical analysis methods of high purity aluminum.Part 3: Determination of titanium content by diantippylmethane-thiocyanate photometric method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本标准规定了工业镓中硅、钠、钾、镁、钙、铝含量的测定方法。 本标准适用于工业镓[99.9%≤ω(%)≤99.995%]中硅、钠、钾、镁、钙、铝含量的测定。测定范围见表1。

Chemical analysis methods of gallium for industrial use.Determination of impurity elements.Inductively coupled plasma atomic emission spectrometric method

ICS
77.120.99
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中铁含量的测定方法。 本部分适用于高纯铝中铁含量的测定。测定范围:0.00010%~0.00050%。

Chemical analysis methods of high purity aluminum.Part 1: Determination of iron content by 1,10-phenanthroline-thiocyanate photometric method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中铁含量的测定方法。 本部分适用于高纯铝中硅含量的测定。测定范围:0.00010%~0.00080%。

Chemical analysis methods of high purity aluminum.Part 2: Determination of silicon content by extraction-molybdenum blue photonEetrie method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中镓含量的测定方法。 本部分适用于高纯铝中镓含量的测定。测定范围:0.00002%~0.00020%。

Chemical analysis methods of high purity aluminum.Part 4: Determination of gallium content by butylrhodamine B photometric method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中铜、锌和铅含量的测定方法。 本部分适用于高纯铝中铜、锌和铅含量的测定。测定范围:铜:0.00005%~0.00050%;锌:0.00002%~0.00050%。铅:0.00003%~0.00060%。

Chemical analysis methods of high purity aluminum.Part 5: Determination of copper, zinc and lead content by anodic spripping Voltammetric method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中银含量的测定方法。 本部分适用于高纯铝中银含量的测定。测定范围:0.00002%~0.00010%。

Chemical analysis methods of high purity aluminum.Part 6: Determination of silver content by eddyze reaction system of manganese-persulfric acid method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中镉含量的测定方法。 本部分适用于高纯铝中镉含量的测定。测定范围:0.00001%~0.00025%。

Chemical andysis methods of high purity aluminum.Part 7: Determination of cadmium content by extraction-dithizone photometric method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中铟含量的测定方法。 本部分适用于高纯铝中铟含量的测定。测定范围:0.00002%~0.00050%。

Chemical analysis methods of high purity aluminum.Part 8: Determination of indium content by extraction-crystal violet photometric method

ICS
77.040.30
CCS
H12
发布
2008-03-12
实施
2008-09-01

本部分规定了高纯铝中铁、钛、镓、铜、锌、铅、铟、镉、银、钴、钼、锑、铋等痕量元素含量的测定方法。 本部分适用于高纯铝(99.999%≤ω(Al)≤99.9995%)中铁、钛、镓、铜、锌、铅、铟、镉、银、钴、钼、锑、铋等痕量元素含量的测定。测定范围见表1。

Chemical analysis methods of high purity aluminum.Part 9: Determination of trace impurities in high purity aluminumby inductively coupled mass spectrometry

ICS
77.040.01
CCS
H12
发布
2008-03-12
实施
2008-09-01

Aluminium and aluminium alloys - Environmental aspects of aluminium products - General guidelines for their inclusion in standards.

ICS
77.150.10
CCS
H12
发布
2008-03-01
实施
2008-03-27

1.1 This specification covers the requirements relating to rinsed and non-rinsed non-hexavalent chromium conversion coatings on aluminum and aluminum alloys intended to give protection against corrosion and as a base for other coatings. 1.2 Aluminum and aluminum alloys are conversion coated in order to retard corrosion; as a base for organic films including paints, plastics, and adhesives; and as a protective coating having a low electrical contact impedance. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory requirements prior to use.

Standard Specification for Non-hexavalent Chromium Conversion Coatings on Aluminum and Aluminum Alloys

ICS
77.120.10 (Aluminium and aluminium alloys)
CCS
H12
发布
2008
实施

This test method for the chemical analysis of metals and alloys is primarily intended to test such materials for compliance with compositional specifications. It is assumed that all those who use this test method will be trained analysts capable of performing common laboratory procedures skillfully and safely. It is expected that work will be performed in a properly equipped laboratory.1.1 This test method covers the chemical analysis of zinc alloys having chemical compositions within the following limits: ElementConcentration Range, % Aluminum 3.0–8.0 Antimony 0.002 max Cadmium 0.025 max Cerium 0.03–0.10 Copper 0.10 max Iron 0.10 max Lanthanum 0.03–0.10 Lead 0.026 max Magnesium 0.05 max Silicon 0.015 max Tin 0.002 max Titanium 0.02 max Zirconium 0.02 max 1.2 Included are procedures for elements in the following concentration ranges: ElementConcentration Range, % Aluminum 3.0–8.0 Cadmium 0.0016–0.025 Cerium 0.005–0.10 Iron 0.0015–0.10 Lanthanum 0.009–0.10 Lead 0.002–0.026 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use. Specific safety hazards statements are given in Section 8, 12.2, and 14.1.

Standard Test Method for Chemical Analysis of Zinc-5 % Aluminum-Mischmetal Alloys by ICP Emission Spectrometry

ICS
77.040.30 (Chemical analysis of metals)
CCS
H12
发布
2008
实施

1.1 This specification covers the requirements relating to rinsed and non-rinsed non-hexavalent chromium conversion coatings on aluminum and aluminum alloys intended to give protection against corrosion and as a base for other coatings. 1.2 Aluminum and aluminum alloys are conversion coated in order to retard corrosion; as a base for organic films including paints, plastics, and adhesives; and as a protective coating having a low electrical contact impedance. 1.3 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory requirements prior to use.

Standard Specification for Non-hexavalent Chromium Conversion Coatings on Aluminum and Aluminum Alloys

ICS
77.120.10 (Aluminium and aluminium alloys)
CCS
H12
发布
2008
实施

이 규격은 강 중의 납 분석 방법에 대하여 규정한다.

Methods for determination of lead in steel

ICS
77.080.40
CCS
H12
发布
2007-09-28
实施
2007-09-28

이 규격은 알루미늄 및 알루미늄합금 제품(이하 제품이라고 한다.)에 성막된 양극 산화 피막

Test methods for corrosion resistance of anodic oxidation coatings on aluminium and aluminium alloys

ICS
77.060;25.220.20
CCS
H12
发布
2007-07-31
实施
2007-07-31

이 규격은 알루미늄 및 알루미늄합금 중 베릴륨 정량방법에 대해 규정한다.

Methods for determination of beryllium in aluminium and aluminium alloys

ICS
77.120.10
CCS
H12
发布
2007-06-29
实施
2007-06-29

이 규격은 마그네슘합금의 규소 분석 방법에 대하여 규정한다.

Determination of silicon in magnesium alloys

ICS
77.120.20;71.040.40
CCS
H12
发布
2007-06-29
实施
2007-06-29



Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号