ISO 11130:2017
金属与合金的腐蚀 盐溶液中的交替浸入试验

Corrosion of metals and alloys - Alternate immersion test in salt solution


标准号
ISO 11130:2017
发布
2017年
发布单位
国际标准化组织
当前最新
ISO 11130:2017
 
 
引用标准
ISO 8044
适用范围
This document specifies a method for assessing the corrosion resistance of metals by an alternate immersion test in salt solution, with or without applied stress. The test is particularly suitable for quality control during the manufacture of metals including aluminium alloys and ferrous materials, and also for assessment purposes during alloy development. Depending upon the chemical composition of the test solution, the test can be used to simulate the corrosive effects of marine splash zones, de-icing fluids and acid salt environments. The term “metal” as used in this document includes metallic materials with or without corrosion protection. This document is applicable to — metals and their alloys, — certain metallic coatings (anodic and cathodic with respect to the substrate), — certain conversion coatings, — certain anodic oxide coating, and — organic coatings on metals.

推荐

一文搞懂腐蚀试验

它是将产品在雾和湿热两种环境条件下交替转换,最后考核整机产品电性能和机械性能有无变化。 GB/T 101254种雾测试方法对比4. 影响因素影响试验结果主要因素包括:试验温湿度、盐溶液浓度、样品放置角度、盐溶液pH值、雾沉降量和喷雾方式等。① 试验温湿度温度和相对湿度影响腐蚀作用。金属腐蚀临界相对湿度大约为70%。...

学术干货 | 你了解金属材料腐蚀检测吗?

它是将产品在雾和湿热两种环境条件下交替转换,最后考核整机产品电性能和机械性能有无变化。图3 GB/T 101254种雾测试方法对比4.4 影响因素影响试验结果主要因素包括:试验温湿度、盐溶液浓度、样品放置角度、盐溶液pH值、雾沉降量和喷雾方式等。1) 试验温湿度 温度和相对湿度影响腐蚀作用。金属腐蚀临界相对湿度大约为70%。...

试验一小时相当于自然环境多少时间?

研究结果表明:钢板水平线成45度角时,每平方米腐蚀失重量为250 g,钢板平面垂直线平行时,腐蚀失重量为每平方米140 g。GB/T 2423.17-93标准规定:平板状样品放置方法,应该使受试面垂直方向成30度角。pH值pH值越低,溶液氢离子浓度越高,酸性越强腐蚀性也越强。中性试验(NSS)  pH值为6.5~7.2。由于受到环境因素影响,盐溶液pH值会发生变化。...


谁引用了ISO 11130:2017 更多引用





Copyright ©2007-2022 ANTPEDIA, All Rights Reserved
京ICP备07018254号 京公网安备1101085018 电信与信息服务业务经营许可证:京ICP证110310号