This specification establishes the requirements for chromate conversion coatings on magnesium alloys. This process has been used typically to improve corrosion resistance and adherence of organic finishes but usage is not limited to such applications. The dichromate treatment may not be suitable for alloys with high manganese content. The chrome pickle treatment has been used as touch-up for previously dichromate-treated surfaces and for improving corrosion protection temporarily, but usages are not limited to such applications.
SAE AMS 2475G-2009由美国机动车工程师协会 US-SAE 发布于 2009-12-18。
SAE AMS 2475G-2009 在中国标准分类中归属于: V10 航空、航天材料基础标准,在国际标准分类中归属于: 49.040 有关航空航天制造用镀涂和有关工艺。
SAE AMS 2475G-2009 镁合金防护处理 由 SAE AMS 2475F-2001 变更而来。