SAE J404-2009
SAE合金钢的化学成分

Chemical Compositions of SAE Alloy Steels


SAE J404-2009



标准号
SAE J404-2009
发布日期
2009年01月27日
实施日期
废止日期
中国标准分类号
H40
国际标准分类号
77.080.20
发布单位
美国机动车工程师协会
引用标准
ASTM A506-2005 ASTM A507-2006 ASTM A513-2008 ASTM A519-2006 SAE J 408-1983 SAE J 409-1995 SAE J 1081-2000 SAE J 1249-2008 SAE J 1268-1995 SAE J 1868-1993
被代替标准
SAE J 404-2000
适用范围
In 1941, the SAE Iron and Steel Division in collaboration with the American Iron and Steel Institute (AISI) made a major change in the method of expressing composition ranges for the SAE steels. The plan, as now applied, is based in general on narrower ladle analysis ranges plus certain product (check) analysis allowances on individual samples, in place of the fixed ranges and limits without tolerances formerly provided for carbon and other elements in SAE steels (reference SAE J408). ISTC Division 1 has developed a procedure which allows for the maintenance of the grade list in this SAE Standard. This will involve conducting an industry-wide survey to solicit input. This survey will be conducted at a frequency deemed necessary by the technical committee. Criteria have been established for the addition to or deletion of grades from the grade table. A new grade will be considered if it meets standard SAE grade ranges, has a minimum usage or production of 225 tonnes/year (250 tons/year), and has the endorsement of at least two users or producers. New steel compositions will still be considered as Potential Standard (PS) steels, based on the guidelines provided in SAE J1081, until such time as production of the new steel achieves a level of production or usage qualifying it for consideration as a standard steel. The deletion of a grade from the grade table will be by consensus based on the grade survey results. Deleted grades will be archived in SAE J1249 for future reference. The compositions in this document may apply to open hearth and basic oxygen, or electric furnace steels. Grades shown in Table 1 with prefix letter E are normally made by the electric furnace process with maximum limits of 0.025% phosphorus and 0.025% sulfur. The nominal chemical limits or ranges in the compositions given in Table 1 are subject to standard variations in check analysis given in SAE J409. Since AISI is no longer issuing steel grade designations, all grades listed in this document are SAE grades.

谁引用了SAE J404-2009 更多引用





Copyright ©2007-2022 ANTPEDIA, All Rights Reserved